Title Tuning electromagnetic absorption for EMI shielding in PBSA composites with Fe3O4-decorated carbon nanotubes
Authors Krikovs, Artis ; Bleija, Miks ; Platnieks, Oskars ; Tsyhanok, Dzmitry ; Banys, Jūras ; Macutkevič, Jan ; Smits, Krisjanis ; Maiorov, Mikhail ; Gaidukovs, Sergejs
DOI 10.1016/j.synthmet.2026.118263
Full Text Download
Is Part of Synthetic metals.. Elsevier B.V.. 2026, vol. 321, art. no. 118263, p. [1-17].. eISSN 0379-6779
Keywords [eng] aqueous co-precipitation ; biodegradable polyester ; conductive-magnetic hybrid nanofillers ; electrical percolation ; impedance matching ; poly(butylene succinate-co-adipate)
Abstract [eng] This study investigates the electromagnetic interference (EMI) shielding behavior of bio-based poly(butylene succinate-co-adipate) (PBSA) composites filled with magnetite (Fe3O4)-grafted single-walled (SWCNT) and multi-walled carbon nanotubes (MWCNT). Hybrid fillers were synthesized via one-step aqueous co-precipitation onto non-functionalized CNTs, yielding nominal Fe3O4 contents of 15 and 30 wt% (actual: 12.1–26.9 wt%), expressed as a fraction of the total filler mass. They were then incorporated into PBSA at 0.10–2.0 vol% via solvent casting. Microscopy revealed two distinct hybrid filler morphologies: individual Fe3O4 nanoparticles dispersed along CNT sidewalls and agglomerates concentrated at CNT junctions. Magnetometry showed that the deposited Fe3O4 was superparamagnetic, with specific magnetization calculated to range from 4.7 to 65 emu/g depending on crystallite size. Tensile testing revealed up to a 2.2-fold increase in elastic modulus and a 1.4-fold increase in ultimate tensile strength. Sheet resistance indicated percolation at ∼ 0.1 vol%, increasing to ∼ 0.5 vol% after Fe3O4 co-precipitation. The composites were analyzed by electromagnetic spectroscopy in the frequency ranges of 0.1–3 GHz and 8.4–12.6 GHz. CNT incorporation produced shielding in which dissipation carried the larger share of the shielding effectiveness, with 〈SEA〉/〈SET〉 ratios of up to 0.78. Fe3O4-grafted MWCNT composites at 1.0 vol% exhibited a broadband absorption plateau below 3 GHz (〈SEA〉/〈SET〉 ratio of 0.70), which the SWCNT-based composites did not develop in this range. Unmodified SWCNT composites at 2.0 vol% transitioned to reflection-dominated shielding at 8.4–12.6 GHz. This work indicates that CNT morphology is an important design variable for absorption-based EMI shielding.
Published Elsevier B.V